铁氟龙, 氟橡胶, 铁氟龙FEP, PVDF法国阿科玛9000HD, ETFE日本旭硝子C-88AX, PFA美国杜邦340, PA66/F/PTFE美国液氮RFL-403, PA66/PTFE美国液氮RL-4040, POM/PTFE基础创新塑料KL004
Fluoroloy® A30 | |||
Polytetrafluoroethylene | |||
Product Description | |||
Material | |||
Glass Formulated PTFE | |||
Features/Benefits | |||
Excellent heat, wear, and chemical resistance. | |||
Good cryogenic properties. | |||
Caution: can be abrasive running against soft metals at high surface speed. | |||
Excellent material for back-up rings. | |||
Working Temperature Range | |||
-450° to +600°F [-268° to +316°c] | |||
Color | |||
Yellow | |||
General | |||
Features | Good Chemical Resistance | Good Wear Resistance | High Heat Resistance |
Appearance | Yellow | ||
Physical | Nominal Value | Unit | Test Method |
Specific Gravity | 2.18 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
Durometer Hardness (Shore D) | 60 | ASTM D2240 | |
Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 427 | MPa | ASTM D4894 |
Tensile Strength | 18.6 | MPa | ASTM D4894 |
Tensile Elongation (Break) | 220 | % | ASTM D4894 |
Compressive Modulus | 883 | MPa | ASTM D695 |
Compressive Strength (1% Strain) | 13.1 | MPa | ASTM D695 |
Coefficient of Friction | 0.09 | Internal Method | |
Deformation Under Load 2 (14 MPa) | 7.2 | % | ASTM D621 |
Thermal | Nominal Value | Unit | Test Method |
CLTE | ASTM E831 | ||
Flow : 26 to 200°C | 1.10E-04 | cm/cm/°C | |
Transverse : 26 to 200°C | 9.90E-05 | cm/cm/°C |